Influence of saliva contamination on zirconia ceramic bonding.

http://www.ncbi.nlm.nih.gov/pubmed/17675146

OBJECTIVES: The purpose of this study was to investigate the influence of saliva contamination and cleaning methods on adhesive bonding to dental zirconia ceramic with a phosphate-monomer-containing luting resin.

METHODS: After saliva immersion, airborne-particle abraded ceramic specimens were cleaned with water rinsing, with isopropanol, with phosphoric acid gel, or with additional airborne-particle abrasion. Airborne-particle abraded specimens without contamination were used as the control group. Chemical analysis of the ceramic surfaces of all groups was done using X-ray photoelectron spectroscopy (XPS). The influence of contamination and cleaning methods on ceramic bond durability was examined by tensile bond strength (TBS) testing after 3 days or 150 days water storage with 37,500 thermal cycles.


RESULTS: After saliva contamination XPS revealed an organic coating which was not removed completely with water rinsing, with isopropanol, or with phosphoric acid. Using TBS testing a strong influence of contamination and cleaning methods on resin bond strength and its durability was found.

SIGNIFICANCE: Saliva contamination significantly affected resin bonds to zirconia ceramic and its durability. Airborne-particle abrasion was the most effective cleaning method.

接着前の汚染物質の除去に Airborne-particle abrasion が有効であると述べてます。
私も接着前に30-50-μm Al2O3などのabrasionを行ってます。
シリカ系のe.maxではどうでしょう?

ウォルセラム ビスケット 小臼歯

2010 年 11 月 9 日

ウォルセラム試適用のビスケット。適合、咬合、マージン、形態をチェック。修正をして完成に進みます。


wolc1 300x188 ウォルセラム ビスケット 小臼歯 wol ceram

wol3 300x185 ウォルセラム ビスケット 小臼歯 wol ceram

wol1 300x192 ウォルセラム ビスケット 小臼歯 wol ceram

型(印象)

2010 年 9 月 15 日

6番オールセラミッククラウンの型です。歯肉の縁まできれいに取ります。セラミックの縁が歯肉の中にわずかに入るので、この部分が正確にとれいると適合が良いものができます。

imp2 300x195 型(印象) wol ceram

imp0 270x300 型(印象) wol ceram